Every sign of failure the Technical Library records under Substructure: 32 signs across 4 elements and spaces. Each row gives what you see, the likely cause and what confirms it, and the next step. Each heading opens the page the rows come from.

Basement, Cellars & Retaining Walls

Water ingress and radon

What you seeLikely cause, and what confirms itNext step
Basement leaks only in wet weatherSurface water reaching the wall. Correlation with rainfall; surface drainage.Fix the surface drainage: regrading, channels and downpipe connections.
Basement leaks all yearGroundwater. Groundwater levels.Inject cracks and joints; where external access is impossible, fit a drained cavity system with sumps and pumps.
High radon result in a basement or cellarGround gas entering through the floor and walls. A long-term test; the US EPA recommends fixing homes at 4 pCi/L (150 Bq/m³) or more (US EPA), and in the UK the risk is relatively low below 100 Bq/m³ (UKradon).Seal entry points and fit a radon sump or ventilation, then retest.

Pressure, rotation and surcharge

What you seeLikely cause, and what confirms itNext step
Retaining wall leaning more after heavy rainBlocked drainage and water pressure. Weep holes and drains inspected.Clear the drains and open the weep holes; keep people and loads away, and get an engineer's assessment.
Wall cracked behind a new driveway or structureSurcharge. Loads against design.Remove the surcharge, or redesign the wall for it.
Inward bowing of cellar wallsLack of restraint and earth pressure. Survey; restraint details.Get an engineer's assessment; restraint, buttresses or anchors.
Cracks in a basement or retaining wall widening between readingsMovement still active. Crack widths read against fixed points over time, and graded on the asset’s market’s damage scale (Thresholds by market).Keep reading the cracks, and have an engineer assess any crack that is still moving or has reached the moderate band.

Timber sleepers and anchors

What you seeLikely cause, and what confirms itNext step
Timber wall leaning with soft postsDecay below ground. Probe posts.Replace the sleeper wall with a concrete or masonry system.

Foundations

Subsidence and heave on clay

What you seeLikely cause, and what confirms itNext step
Diagonal cracks widening toward the top at one corner, near a large treeSubsidence from clay shrinkage. Seasonal crack opening; soil moisture and root analysis; crack widths graded on the asset’s market’s damage scale (Thresholds by market).Find the cause, usually a tree or a leak; remove it, then monitor before deciding on underpinning.
Cracks widening in summer and closing in winterSeasonal clay movement. Twelve months of crack monitoring.Monitor for twelve months; manage trees and drainage; repair the cracks once stable.
Floors lifting in the middle, cracks wider at the top of internal wallsHeave after tree removal or leaks. Level survey; history of tree removal.Survey the levels and stop any leaks; assess heave before any further tree removal.

Settlement, washout and chemical attack

What you seeLikely cause, and what confirms itNext step
Sudden local drop near a drain runWashout from a leaking drain. Drain CCTV; void detection.Repair the drain, then stabilise the ground, by underpinning or resin injection if needed.
Crack between extension and original buildingDifferent foundations moving differently. Foundation depths; level survey.Establish both foundation depths and monitor; underpin only if movement continues.
Floors out of level across an internal wall lineDifferential movement of the footings. Level survey with a straight edge, graded on the asset’s market’s floor scale (Thresholds by market).Map the levels and find the cause, then monitor before deciding on underpinning.

Timber piles and stumps

What you seeLikely cause, and what confirms itNext step
Uneven floors in a house on timber stumpsDecayed or sunken stumps. Sub-floor inspection.Restump with concrete or steel stumps, and re-level the floors.

Mine subsidence and earthquakes

What you seeLikely cause, and what confirms itNext step
Building tilting slowly over a wide areaMine subsidence or regional settlement. Mining records; survey.Check the mining records and survey; in mine subsidence districts, claim through the relevant scheme.

Slab on Ground

Cracking, curling and settlement

What you seeLikely cause, and what confirms itNext step
Fine random cracks, no displacementDrying shrinkage. Pattern; age; stability.No structural repair; route and seal them where they affect finishes.
Panel corners rocking at jointsCurling. Level survey across joints.Grout under the lifted panels and grind the high edges.
Slab dished near the centre or edges droppingSettlement or clay shrinkage. Level survey and soil investigation, with offsets graded on the asset’s market’s floor scale (Thresholds by market).Investigate the soil; lift and stabilise by injection, or manage the loads.
Racking leaningFloor out of level or settlement under baseplates. Survey.Survey the floor; add baseplates, relocate the racking, or stabilise the slab.
Cracks in a house slab that have opened over a yearMovement beyond drying shrinkage. Crack width graded on the asset’s market’s slab scale (Thresholds by market).Monitor widths and levels, and have an engineer assess cracks in the moderate band or above.

Joints, surface wear and post-tensioning

What you seeLikely cause, and what confirms itNext step
Broken joint edges in forklift aislesWheel impact on open joints. Joint width; forklift wheel type.Rebuild the arrises; install armoured joints in heavy-traffic aisles.

Moisture, flooring and termites

What you seeLikely cause, and what confirms itNext step
Floor finish blistering or debondingMoisture vapour through the slab. In-situ relative humidity testing.Test the slab's relative humidity; lay a surface membrane before new flooring.
New flooring planned over a recent or damp slabSlab moisture not yet tested. In-situ relative humidity probes to ASTM F2170, read against the limit the flooring manufacturer sets.Test before laying; use a moisture-tolerant system or a surface membrane where the reading exceeds the limit.

Sub-floor & Crawlspace

Wet rot and dry rot

What you seeLikely cause, and what confirms itNext step
Soft joist ends at external wallsWet rot from damp walls or blocked vents. Moisture readings.Clear the vents and lower the ground levels; replace the decayed timber.
White strands across masonry and fruiting bodiesDry rot. Identification.Remove the moisture source; cut out affected timber well beyond the visible damage, and treat the masonry.
Damp ground or standing water under the floorWater reaching the sub-floor. Inspection after rain; ground falls; downpipe and plumbing discharge.Regrade, connect downpipes, fix leaks, and lay a ground membrane where the ground stays damp.

Termites and stumps

What you seeLikely cause, and what confirms itNext step
Uneven floors in a house on timber stumpsDecayed or sunken stumps. Sub-floor inspection.Restump, and replace decayed bearers and joists.
Hollow timbers with mudTermites. Inspection; termite detection.Treat with chemical barriers or baiting, fix ant caps and remove bridges; replace damaged timber.
Floor framing close to the groundNo room to ventilate or inspect. Ground clearance under the lowest member against the asset’s market (Thresholds by market).Lower the ground or improve access, and keep the clearance clear of stored material.

Services, ventilation and radon

What you seeLikely cause, and what confirms itNext step
Musty smell and mouldPoor ventilation or damp ground. Humidity and ventilation check, with vent area against the asset’s market (Thresholds by market).Clear and add vents, lay a ground vapour barrier, or add mechanical ventilation.